MEMSnet Home: MEMS-Talk: SPR 220-3 Au plating problem
SPR 220-3 Au plating problem
2005-07-12
Mehmet Unlu
2005-07-12
Tolga Kaya
SPR 220-3 Au plating problem
Tolga Kaya
2005-07-12
Mehmet, I am using SPR 220-7 instead of SJR 5740 as a photoresist. I
know that SPR reflows if you hard-bake it above 100degrees Celsius.
Have you tried it without hardbake? SPR is pretty stable.

Tolga

On 7/12/05, Mehmet Unlu  wrote:
> Hi everyone,
> we are trying to replace SJR 5740 with SPR 220-3 for electroplating
> process. However we observed that SPR220 can not withstand inside the
> cyanide gold plating solution even for a hardbake temperature of 120 C
> for 12 hours.  For SJR 5740, we managed to achieve very stable features
> for a plating duration of 30 minutes. The hardbake temperature for SJR
> 5740 is 80 C for 12 hours. Do you have any experience about the
> durability of SPR 220-3? Do you have any alternatives to be used as mold
> photoresist for 30-40 minutes of gold plating?
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
The Branford Group
Mentor Graphics Corporation
Tanner EDA by Mentor Graphics