Jesse D Fowler
2005-07-14
Here's what I know about ITO etching.

I used 5%HNO3, 20%HCl, 75%DI water (by volume) at about 60 deg.C. My etch times
varied. I suspect it was a combination of factors, those being: 1. My ITO was
not consistent from piece to piece (I could not batch etch), and 2. The etch
product affects the etchant.

PR (AZ 5124) was OK in the etchant until it started to turn green, then would
rapidly strip off.

This etch process takes a lot of attention. If you can find a more stable
process, you should try that.

Jesse Fowler
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Nano-Master, Inc.
MEMS Technology Review
Tanner EDA by Mentor Graphics