A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: About the Piranha cleaning
About the Piranha cleaning
2005-07-14
Zhiwei Zou
2005-07-14
Sumant Sood
2005-07-14
Hongjun-ECE
2005-07-15
Zhiwei Zou
2005-07-15
Brent Garber
2005-07-15
Jesse D Fowler
2005-07-15
Sumant Sood
2005-07-15
Barry Isenor
2005-07-15
Virginia Abranches de Sousa R. Soares
2005-07-15
Shile
2005-07-15
Gary
About the Piranha cleaning
Sumant Sood
2005-07-15
Zeng,

I have been using Piranha etch with H2O2 added to H2SO4 and its not
dangerous if used in the right ratio and concentration. I am citing some
links from the web which recommend adding H2O2 to H2SO4 and not the other
way round. As is widely known, adding water to concentrated H2SO4 is
dangerous but adding the right concentration of H2O2 (30% by vol.) though
exothermic, is a controlled reaction.


http://www.boldtech1.com/technical/piranha_etch.html

http://www.enma.umd.edu/LAMP/Sop/Piranha_SOP.htm

But I might be missing something and would like to hear from others who do
use Piranha as to what their procedure is.

Thanks
Sumant
Belford Research


-----Original Message-----
From: Hongjun-ECE
Subject: RE: [mems-talk] About the Piranha cleaning

Belford,

Please confirm that it is H2So4 added to H2O2, instead of H2O2 added to
H2So4, which might be dangerous.
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics
Addison Engineering
The Branford Group