2005-07-14
Zhiwei Zou
2005-07-14
Sumant Sood
2005-07-14
Hongjun-ECE
2005-07-15
Zhiwei Zou
2005-07-15
Brent Garber
2005-07-15
Jesse D Fowler
2005-07-15
Sumant Sood
2005-07-15
Barry Isenor
2005-07-15
Virginia Abranches de Sousa R. Soares
2005-07-15
Shile
2005-07-15
Gary
About the Piranha cleaning
Brent Garber
2005-07-15
Zhiwei,

We had a large bath of H2SO4 we kept on a hot plate all week long for batch
dipping Si wafers.  We had to add H2O2 every morning before heat it up.
There is the order I used for years.

Hope this helps and don't get any on you!

Brent

Zhiwei Zou wrote:

>
> I am confused about the sequence of mixing these two chemicals. Some
> materials said add H2O2 to H2SO4 but others do it reversely.
> Who can help me to confirm it?
>
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
Nano-Master, Inc.
Tanner EDA by Mentor Graphics
Mentor Graphics Corporation