Hi Simon.
Most folks would probably argue that SAMs are usually applied as a langmuir-
blodgett (sp?) film. The vapor deposition of silane, such as Bill Moffet
mentioned will give you a covalent bond to the glass (via SiO2), and allow you
to put any functional group 'up top'...away from the glass. I think these will
be more robust than the SAM approach.
Best,
Jim Clements

-----Original Message-----
From: [email protected]
[mailto:[email protected]]On Behalf Of Simon Garcia
Sent: Monday, July 18, 2005 10:36 PM
To: General MEMS discussion
Subject: [mems-talk] Stability of silane-based SAMs


Hello,

I would like to functionalize a SiO2/Si or glass surface to improve
film deposition of metal oxides on the substrate. I think SAMs based on
organosilicon molecules, is the best way to go. The problem is that my
film deposition occurs in H2O, at pH=10 and temperature of 75 deg C,
and I'm afraid the basic conditions will attack the monolayer.

Does anyone have experience with organosilane monlayers, and had
problems with stability in aqueous solution?

Where can I find studies on the stability of these monolayers in
different environments?
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
The Branford Group
Harrick Plasma, Inc.
MEMStaff Inc.