D. Zhou
2005-07-22
PRAMOD GUPTA
high melting-point wax used in KOH etch
PRAMOD GUPTA
2005-07-22
Brewer Science is developing a material that meets your description: a
spin applied material, cured at under 250 degrees Celsius, able to withstand
8 or more hours of 85 degree Celsius KOH (35%).  This material is removed
with standard photoresist removal process.

"D. Zhou"  wrote:Dear all,

Does anyone know where I can get some high melting-point wax which can be
used to protect the device side of the chip when doing KOH etch at 80
degrees to remove the substrate ? Many thanks.


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
MEMS Technology Review
Tanner EDA by Mentor Graphics
Harrick Plasma, Inc.