MEMSnet Home: MEMS-Talk: PDMS bonds to silicion wafer?
Black spots on PDMS!!!
2005-07-19
Vishwanath Somashekar
Re: Black spots on PDMS!!!
2005-07-22
Marc Hennemeyer
PDMS bonds to silicion wafer?
2005-07-27
[email protected]
2005-07-28
Cheng Ming Lin
PDMS bonds to silicion wafer?
Cheng Ming Lin
2005-07-28
Dear ,

PDMS can be bond with PDMS, glass and Si after the treatment of oxygen
plasma. ( You can use plasma cleaner or RIE )

C.M. Lin
NTU, Taiwan, R.O.C

-----Original Message-----
From: [email protected] [mailto:[email protected]]
Sent: Wednesday, July 27, 2005 12:16 PM
To: General MEMS discussion
Subject: [mems-talk] PDMS bonds to silicion wafer?

Hello all,

Recently people are discussing about bonding between PDMS and glass and
bonding between PDMS and PDMS.
I am wondering anyone has experience of bonding between cured PDMS and
silicon?
Thanks,

chengsheng


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Addison Engineering
MEMS Technology Review
Nano-Master, Inc.