Prasad Mohan Lotlikar
2005-07-29
shay kaplan
pdms impermeable coating?
Prasad Mohan Lotlikar
2005-07-29
hi all,
I am working on a micropump design and am using 100 um thick PDMS slygard
diaphragm as actuation valve to pump water. Now since PDMS is permeable to
moisture I need to coat another thin impermeable layer on it.
the properties of this second layer must be-
it must be flexible (so that pdms deflection is not compensated)
it must be transparent or optically clear
thin and easily available.

can anyone help or suggest me the solution to this problem??

thanks in advance,
Prasad.
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
University Wafer
Tanner EDA by Mentor Graphics
The Branford Group