Prasad Mohan Lotlikar
2005-07-29
shay kaplan
pdms impermeable coating?
shay kaplan
2005-07-29
Try to deposit Parylene C

-----Original Message-----
From: [email protected] [mailto:[email protected]]
On Behalf Of Prasad Mohan Lotlikar
Sent: Friday, July 29, 2005 3:17 AM
To: [email protected]
Subject: [mems-talk] pdms impermeable coating?

hi all,
I am working on a micropump design and am using 100 um thick PDMS slygard
diaphragm as actuation valve to pump water. Now since PDMS is permeable to
moisture I need to coat another thin impermeable layer on it.
the properties of this second layer must be-
it must be flexible (so that pdms deflection is not compensated)
it must be transparent or optically clear
thin and easily available.

can anyone help or suggest me the solution to this problem??
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
The Branford Group
Mentor Graphics Corporation
MEMStaff Inc.