MEMSnet Home: MEMS-Talk: How to etch Silicon into oblique walls using ICP?
Pyrex wafer anodically bonded to Thin Silicon Problem
2005-08-01
Zoberbier, Margarete
2005-08-01
Tony Rogers
Coating of Poly Si with a Ferromag Matl !!!!
2005-08-01
Namit Singh
How to etch Silicon into oblique walls using ICP?
2005-08-01
ning
2005-08-01
Hongjun-ECE
2005-08-02
ning
2005-08-03
David Nemeth
How to etch Silicon into oblique walls using ICP?
ning
2005-08-01
Hi everyone,

Common goals of using ICP etching is to form vertical walls. But what I need
to do is just the opposite. We want to etch in Silicon wafer some deep
trenches with an oblique angle about 45 degree. And we want the etch rate to
be as fast as possible.
I am completely new to this topic, I really need some advice.
Thanks.
Ning

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Addison Engineering
Nano-Master, Inc.
University Wafer