Hello.  I am looking for someone to perform a lapping process on a wafer I
have plated with nickel on top of thick photoresist.

I am also looking for a used diamond saw system for dicing silicon wafers,
that is for sale.

Robert Dean
RF CMOS Designer
MEMS Optical
205 Import Circle
Suite 2
Huntsville, AL 35806
Tel. 205-859-1886
FAX 205-859-5890
email [email protected]