SU-8 UV degradation
[email protected]
2005-08-02
Greetings,
I don't believe there is a UV problem.
We developed finger print ID devices that had a final coating of SU8 ,we
found no degradation during testing to my knowledge.
Regards
walter
www.elume.com

-----Original Message-----
From: Michael L [mailto:[email protected]]
Sent: Tuesday, August 02, 2005 1:35 AM
To: [email protected]
Subject: [mems-talk] SU-8 UV degradation

Hi,

Does anyone know if SU-8 undergoes UV degradation during prolonged exposure
after crosslinking? Polymers generally exhibit such an effect but the same
may not be true for epoxy class polymers. Any information would be
appreciated.

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Addison Engineering
MEMStaff Inc.
MEMS Technology Review