MEMSnet Home: MEMS-Talk: SiO2 over gold
ANSYS command for deposition
2005-08-02
maryala shivakumar
SiO2 over gold
2005-08-03
mojgan daneshmand
2005-08-03
Richard Chang
2005-08-04
Jesse D Fowler
2005-08-03
Guillermo Villanueva
SiO2 over gold
Richard Chang
2005-08-03
Hi,

   Do you have adhesive layer between SiO2 and gold?
   I used to have sputtering SiO2 on top of gold.
   My experience is if you have too thick adhesive layer, more than 30 nm,
it's easy to crack when you are doing post-process.
   Wish that help.

Richard

----- Original Message -----
From: "mojgan daneshmand" 
To: "General MEMS discussion" 
Sent: Tuesday, August 02, 2005 7:49 PM
Subject: [mems-talk] SiO2 over gold


> Hi everyone,
>
> I am having problem with PECVD SiO2 over gold film. Our oxide film looks
> perfectly fine over any surface rather than gold. It cracks over any gold
> pattern. Has anyone seen any similar problem? any idea how I can fix the
> problem?
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Tanner EDA by Mentor Graphics
Addison Engineering
University Wafer