A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: any special trick for taking SEM of PDMS
any special trick for taking SEM of PDMS
2005-08-03
[email protected]
2005-08-04
abong
2005-08-16
Woo-Jin Chang
2005-08-16
Cristi Lepadatu
2005-08-17
Scott Walck
2005-08-17
Cristi Lepadatu
2005-08-19
Isaac Wing Tak Chan
any special trick for taking SEM of PDMS
abong
2005-08-04
it's hard to see PDMS..

as a matter of fact on all dielectric material..


On Wed, 3 Aug 2005 [email protected] wrote:

> Hello,
>
> I'm having difficulty taking SEM for PDMS.
> I coat a thin layer of gold about 150A on PDMS.
> However the SEM resolution is so low for some reason. I took the SEM for the
> master, which is photoresist. I can see 0.25um feature. However for PDMS, the
> image is blur even for 10um feature. I am just wondering if I miss something.
> Or it just hard to see PDMS.
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
Nano-Master, Inc.
Tanner EDA by Mentor Graphics
University Wafer