A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Photoresist for Lift-off process
Photoresist for Lift-off process
2005-08-02
Richard Chang
2005-08-03
Bill Moffat
2005-08-05
Brubaker Chad
2005-08-08
Huy Vo
KOH Wet Etching of Si wafers
2005-08-09
Daniel Park
2005-08-10
Shay Kaplan
2005-08-12
Christian Schröder
2005-08-12
Josef Kouba
2005-08-09
Wilson, Thomas
2005-08-11
Boyd Evans
Photoresist for Lift-off process
Brubaker Chad
2005-08-05
With he resists you list, lift-off would be difficult, since all of them
will exhibit a positive slope profile.  Also, all of those materials are
of the same, or similar, resin chemistry, so performing a two-stage
develop to create an undercut profile is not an option either.

Some suggestions for processing (which would require additional
materials, of course):

1) Use a lift off resist (negative tone) such as AZ nLOF 2000 series
(uses similar chemistry to AZP4620, and so can be processed in the same
spin bowl).

2) Use an image reversal resist (such as AZ 5214) - this can also give a
good negative profile for lift-off. Also, YES (Yield Engineering
Systems) has a solution for lift-off processes with other resists
(search the mems-talk archives for more info).

3) As I mention above, try to use a binary system, such as a PMGI
underlayer (from MicroChem), with resist over the top.  This way, the
top layer of resist will not directly interact with the bottom layer,
and the bottom layer will be undercut during the develop process.

Best Regards,
Chad Brubaker

-----Original Message-----
From:  Richard Chang
Subject: [mems-talk] Photoresist for Lift-off process

Hi, All,

  Does anybody know what the photoresist are for lift-off process other
than Futurrex NR7-1500PY?
  I need to use lift-off process to pattern the sputtering silicon
dioixde layer. But I don't have NR7-1500 PY.
  Could I use two different photoresists, just normal positive
photoresists, to do the lift-off? I have S1813, AZP 4620, and AZP 4210.
  Is there guidance I should follow?
  Thanks.
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
The Branford Group
Tanner EDA by Mentor Graphics
Addison Engineering