laser interference lithography
2005-08-05
Cheng Lu
2005-08-08
Fred Chen
laser interference lithography
Fred Chen
2005-08-08
Cheng,

Generally for a line-space interference pattern you want the polarization
parallel to the lines.

Regards,
Fred

----- Original Message -----
From: "Cheng Lu" 
Subject: [mems-talk] laser interference lithography

> I am doing the three beam laser interference lithography with 355nm laser.
> My problem is that resulted pattern was partially interferenced. This
> becomes more obvious when the period goes to the smaller values like
> 400nm. I know here the polarization and distance is very important. The
> distance I am sure that was controlled very well. But for the
> polarization, I am not sure how can I set the best value, for example, the
> co-angle setting at 45 degree.
>
> Is there anybody who could give me any suggestion on how to work it out?
>
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics
University Wafer
Addison Engineering