Dear All,

I have etched 20-25 micron wide and 450-500 um deep holes in silicon
wafer by DRIE process. Now, i have to cut them along the center of the
holes so that i can take the SEM pictures of their cross section.
Right now, i am cutting them manually (by simple diamond cutter) but
till now i am not able to cut them perfectly.

Can any body suggest any method, how i can cut such deep holes along
the diameter.

--
Thanks,
Pradeep Dixit
Research Student,
Micromachine Center,
NTU Singapore - 639669
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing
MEMS Technology Review
Addison Engineering