Lift-Off-Process question
2005-08-10
Sven Passinger
2005-08-10
Jesse D Fowler
2005-08-10
Cristi Lepadatu
2005-08-11
Sven Passinger
2005-08-11
William Lanford-Crick
eutectic point of silicon-aluminum
2005-08-11
li cai
2005-08-12
Felix Lu
2005-08-11
Guillermo Villanueva
2005-08-11
Sven Passinger
2005-08-11
[email protected]
Lift-Off-Process question
Guillermo Villanueva
2005-08-11
I'm not sure I totally understood you, but just to be sure:
Have you taken into account that when making photolithography on glass it is
very difficult to assure if you are well focussed on the surface or not?

We had some problems with that in our center and we finally gave up trying
to obtain very small features.

Regards,

Guillermo Villanueva
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Harrick Plasma, Inc.
MEMStaff Inc.
University Wafer