You can read the paper by J.O McCaldin and H.Sankur "Diffusivity and solubility
of Si in the Al metallization of integrated circuits Appl Phys Lett 19(1971)
524..

 according to the paper the diffusivity of Si in Al @ 400 deg C is approx
10um*2/min

Rakesh

Bill Moffat  wrote:
I do not know the eutectic point. I do know that in at least 5
different semiconductor manufacturers I worked in we alloyed aluminum to
silicon at about 435 degree C in a reducing atmosphere. It led to the
manufacture of our 450 degree C oven with reducing gas control.
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Tanner EDA by Mentor Graphics
MEMStaff Inc.
University Wafer