MEMSnet Home: MEMS-Talk: RE: Need properites of Single Crystal Silicon
RE: Need properites of Single Crystal Silicon
2005-08-17
Zhang Xuming
2005-08-18
Roger Brennan
RE: Need properites of Single Crystal Silicon
Roger Brennan
2005-08-18
Just a gentle reminder.  Extended baking at 400C or so can produce thermal
donors in CZ silicon (tend to go n-type).  30 minutes apparently is no
problem but think twice before going several hours.

Roger Brennan

-----Original Message-----
From: Zhang Xuming
Sent: Wednesday, August 17, 2005 2:27 AM
To: [email protected]
Subject: [mems-talk] RE: Need properites of Single Crystal Silicon


Hi Anwar:

For bulky silicon, the poisson's ratio is 0.22 - 0.27, thermal conductivity
1.3 W cm-1°C-1, Thermal expansion coefficient 2.6·10-6°C -1.
Cannot find the
value of Jeta.

You may refer to http://www.memsnet.org/material/siliconsibulk/ and
http://www.ioffe.rssi.ru/SVA/NSM/Semicond/Si/index.html for more data and
more references.
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
The Branford Group
MEMS Technology Review
Nano-Master, Inc.