Mac,
Can they use 0.25N KOH or NaOH?

shay

-----Original Message-----
From: Mac Daily
Sent: Thursday, August 18, 2005 10:57 PM
To: MEMS discussion
Subject: [mems-talk] G line positive resist - non TMAH developer

Hello Everyone,

Can anyone recommend a positive tone, G-line photoresist that does not use
TMAH as the developer.  I have a customer that needs such a material and we
don't manufacture one.
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Addison Engineering
Process Variations in Microsystems Manufacturing
Harrick Plasma, Inc.