Polyimide etch
2005-07-25
kris
2005-08-22
kris
Polyimide etch
kris
2005-08-22
Hello All,

I am trying to etch PI2611 of about 14 microns over
the gold bond pads. The bondpads were electroplated. I
am using Al mask for the polyimide etch. After the
etch i have observed that the strings of polyimide
coming off along the preiphery of the bond pads. These
strings appear to be thinner compared to the original
polyimide layer. I was wondering if anyone has
encountered similar kind of problems??

Please provide me any suggestions on this.

Thanks
Kris
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Harrick Plasma, Inc.
The Branford Group
Process Variations in Microsystems Manufacturing