Hi,

I have used the same process as you require--Electroplating Ni on Cu/Cr and
etching Cu/Cr with nickel intact. Use Nanostrip to selectively etch Cu/Cr
without etching Ni. It does a very good job.Took me around 2-3 mins for
200nm of Cu on 50nm of Cr.

regards
Rajib