Hi,

I used an ammonium peroxydisulfate as selective etchant of copper in order to
release my electrodeposited nickel.
The first time, it worked very well

Now, with some change in the bath composition, and current density applied, I
find that nickel etches very quickly. I suppose then that either one element in
my bath or the microstructure of the nickel has a big effect on the competition
between the etching rate of copper and nickel

but maybe you have some more clever thoughts about that?


Dr Laetitia Philippe
Electrochemistry and Micro-patterning Group
EMPA

>>> [email protected] 08/30 10:25 pm >>>
Hi,

I have used the same process as you require--Electroplating Ni on Cu/Cr and
etching Cu/Cr with nickel intact. Use Nanostrip to selectively etch Cu/Cr
without etching Ni. It does a very good job.Took me around 2-3 mins for
200nm of Cu on 50nm of Cr.
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Harrick Plasma, Inc.
The Branford Group
Addison Engineering