Hi all,

  I am fabricating a typical transistor recently. But, due to the
unavailability of the SiO2 deposition system, I use SiO2 as an dielectric
layer. So, I am looking for other alternatives. I think the only process I
can do is spinning or thermal evaporation. I am thinking of spin-on-glass
(SOG). Do you guys have experience on this and would like to kindly sharing
with me? Also, do you have any other alternatives?
Thank you so much.
  Looking forward to hear you.

Best regards,
Hoyin
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Harrick Plasma, Inc.
MEMStaff Inc.
MEMS Technology Review