A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: MEMS switch contact dimple
MEMS switch contact dimple
2005-08-31
erkin seker
2005-09-01
Phillipe Tabada
2005-09-01
David Nemeth
Surface Planarization
2005-09-05
erkin seker
2005-09-01
Lou Chomas
2005-09-01
[email protected]
2005-09-01
Bill Moffat
MEMS switch contact dimple
Phillipe Tabada
2005-09-01
Hi Erkin

  Look up processes involving UV hardening your PR and then placing it under
elevated temperatures in order to crosslink the polymers.  This should
prevent the first layer of PR from dissolving when the second layer of PR is
deposited.

Phil Tabada

>From: "erkin seker" 
>Subject: [mems-talk] MEMS switch contact dimple
>Date: Wed, 31 Aug 2005 09:46:31 -0400
>
>Hi,
>
>I am trying to build MEMS DC switches using both cantilevers and bridges.
>I want to fabricate a contact dimple using a bilayer photoresist process.
>I could get the dimple topography I wanted on the sacrificial layer by
>consecutively spinning and patterning two layers of AZ4110 in the past.
>However, now when I spin the second layer, it seems to dissolve the first
>layer where the dimple indentation is.
>
>Does anybody have a relatively straight-forwards recipe for fabricating
>contact dimples?
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
Nano-Master, Inc.
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing