MEMSnet Home: MEMS-Talk: Poor adhesion between Ag and Si
Poor adhesion between Ag and Si
2005-09-07
wangx
2005-09-07
Shay Kaplan
2005-09-07
Hongjun-ECE
2005-09-13
Zeta Tak For YU
Poor adhesion between Ag and Si
wangx
2005-09-07
Dear MEMS community:
Could any of you give me some suggestion on how to improve the adhesion
between Ag and Si? I tried  a thin layer of Cr or Ti by PVD, but it did
not really work, cause the Ag layer peeled off easily when i did some
electrochemical experiment. Could you give me some detailed information
or parameters, if you have the corresponding experiences. Thanks in
advance!

Best Regards

Xuemei Wang
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Tanner EDA by Mentor Graphics
University Wafer
MEMStaff Inc.