PMMA dilution in chlorobenzene
2005-10-13
Noemi Graziana SPARTA'
2005-10-13
William Lanford-Crick
2005-10-13
Fabio Altomare
PMMA dilution in chlorobenzene
Fabio Altomare
2005-10-13
Noemi,

 in our lab we normally start from PMMA 8% and we dilute that to 4%. After
spinning and curing the dilution, we obtain a final thickness of ~180 nm.
We have also diluted down to 2% without any trouble.
Let me know if you have any question.

 Fabio


On Thu, 13 Oct 2005, Noemi Graziana SPARTA' wrote:

> Dear all,
>
> I'm starting to work on PMMA 950K 9%.I'd like to reduce viscosity to
> operate with a thickness (after spin coating) in the range of
> 100-200nm.I'd like to know if the procedure of dilution in chloro
> benzene is a good solution or if it's raccomended to buy a new bottle
> with proper viscosity.
>
> Thanks in advance
> Noemi
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Process Variations in Microsystems Manufacturing
Nano-Master, Inc.
Tanner EDA by Mentor Graphics