MEMSnet Home: MEMS-Talk: problems with AZ 1518 (or AZ 1512 HS) photoresist
problems with AZ 1518 (or AZ 1512 HS) photoresist
2005-10-14
Adrian S.
problems with AZ 1518 (or AZ 1512 HS) photoresist
Adrian S.
2005-10-14
In our work we have the following situation:

-we used AZ 1518 (or AZ 1512 HS) photoresist
(MicroChemicals GmbH) and AZ 400k developer for
lithographic process.

-for wet etching of Ni film we used 20% HNO3 solution
(and others) that causes damages of  Sb deposited film
protected with photoresist.

Please send us your recommendations about using of
these photoresists in wet etching process of Ni film.

Thank you
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Harrick Plasma, Inc.
The Branford Group
Process Variations in Microsystems Manufacturing