MEMSnet Home: MEMS-Talk: testing of a diaphragm
testing of a diaphragm
2005-10-25
Abhay C. Deshpande _04307411_
2005-10-26
Shay Kaplan
testing of a diaphragm
Abhay C. Deshpande _04307411_
2005-10-25
hello everyone,
  i have made a diaphragm by using single polished wafer. i need to test
the diaphragm. i want to test the diaphragm by applying point load at
the center from the front side. please advice me on how to pinpoint the
center of the diaphragm for applying the load.

thanks and regards
abhay

reply