Drill and tap some small holes and make your own clips out of RF strapping
material.  I could send you photos if you want to contact me.  I have the same
system.

Brent

áÎÄÒÅÊ
ôËÁÞÅÎËÏ wrote:

>  Hi,
> Could somebody let me know about standard wafer holder for Balzers BAS450? I
have smooth vertical surface without any tapping holes. How should I  attach 2
inch wafer to it?
>  Thank you in advance,
>  Andrey.
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
Tanner EDA by Mentor Graphics
MEMS Technology Review
Process Variations in Microsystems Manufacturing