Ni etchant
2005-10-31
Prem Pal
2005-10-31
adnan merhaba
Ni etchant
adnan merhaba
2005-10-31
Prem,

Try Ni-etchant TFG from Transene. It has high
selectivity with Copper (sputtered or plated). Here is
the link for more information:
http://www.transene.com/ni_etchant.html

Regards,
Adnan Merhaba


--- Prem  Pal  wrote:

>
> Dear researchers
> Is there any Ni-etchant solution which has high
> selectivity with sputtered Copper (Cu) metal.
>
> Any kind of suggetions will be highly appreciated.
> Thanks in advance
>
> Best regards
> Prem
> _______________________________________________
> Hosted by the MEMS and Nanotechnology Exchange, the
> country's leading
> provider of MEMS and Nanotechnology design and
> fabrication services.
> Visit us at http://www.mems-exchange.org
>
> Want to advertise to this community?  See
> http://www.memsnet.org
>
> To unsubscribe:
>
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
>


__________________________________________________
Do You Yahoo!?
Tired of spam?  Yahoo! Mail has the best spam protection around
http://mail.yahoo.com
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Nano-Master, Inc.
Mentor Graphics Corporation
Addison Engineering