A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: What's the chemical content of the AZ developer?
What's the chemical content of the AZ developer?
2005-11-03
Jeff chen
2005-11-03
Robert Black
surface energy interface silicon-silica
2005-11-03
Giuliano Gregori
2005-11-04
Tim Dellinger
2005-11-03
Brubaker Chad
What's the chemical content of the AZ developer?
Brubaker Chad
2005-11-03
Jifeng,

That depends on the developer that is being used.  The two most commont
are AZ300MIF (a .26N - 2.38% - TMAH solution in water) and AZ400K (a KOH
based developer).

Best Regards,
Chad Brubaker


-----Original Message-----
From: Jeff chen
Sent: Thursday, November 03, 2005 9:16 AM
To: [email protected]
Subject: [mems-talk] What's the chemical content of the AZ developer?

Hi, all,

I am working on a project that needs to modify the silicon surface.
Firstly I have a layer coated on the wafer, then spin coat AZ 1518 to
do the lithography. After useing AZ developer, I found the bottom
layer has some defects.
Anyone knows the chemical content of the AZ developer?
Does it deactivate the amin group?
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
The Branford Group
MEMS Technology Review
Harrick Plasma, Inc.