Yu, Keven
2005-11-07
You can use photoresist AZ 4620 or similar PR, pattern and bake at 140C for 2
min on hotplate.  Then you can deposit metal seed layer.  Second layer
photoresist on metal should be softbake as regular temperature 90 to 105C.

Regards,
-Keven

-----Original Message-----
From: Giuliano Gregori
Sent: Monday, November 07, 2005 11:08 AM
To: General MEMS discussion
Subject: [mems-talk] HD-8820 Polyimide

Hi all,
I'd like to use polyimide as sacrificial layer for the fabrication of an
air-bridge.
I'll have to spin it on a SiO2 surface; on part of the top I'll have to
deposit gold and SiO2 again.
I was thinking to use HD-8820 polyimide and I wonder whether this is a
good solution.
Has anybody already used something similar ?   Suggestions ???
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation