MEMSnet Home: MEMS-Talk: Lift off for oxide mask?
Lift off for oxide mask?
2005-11-07
Pete Kirby
2005-11-08
William Lanford-Crick
Lift off for oxide mask?
Pete Kirby
2005-11-07
Hi-

I was wondering if it is possible to do some sort of lift off process for
creating and oxide mask (2-3 um thick). I found wet etch do be terrible for
accuracy and we have been experiencing problems with our plasma etch
process for some time.

Just looking for an alternative. I am told it can not be done, but I figure
maybe some one may have tried it.

Thanks
Pete

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Mentor Graphics Corporation
The Branford Group
MEMStaff Inc.