Hi Michaela,

a good overview of the influence on SiO2-surfaces by
different cleaning procedures is described by P.
Mueller-Buschbaum in:
"Influence of surface cleaning on dewetting of thin
polystyrene films"
Eur. Phys. J. E 12, 443–448 (2003)
There are two procedures described yielding
SiO2-surfaces with contact angle against water below
2°.

Best regards

Harald




> > Von: "Wullinger, Michaela"
> 
> An: 
> Datum: Mon, 7 Nov 2005 18:04:58 +0100
> Betreff: [mems-talk] SiO2 hydrophilic enhanced?
>
> hi all,
> I'm thinking about ways to make SiO2 more
> hydrophilic.
> What do you think about:
> *HMDS?
> *Temperature (heating)
> *Other promoter?
>
> Any hint is welcome
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Addison Engineering
MEMS Technology Review
Harrick Plasma, Inc.