MEMSnet Home: MEMS-Talk: Ti etchant but not etch SiO2
Ti etchant but not etch SiO2
2005-11-17
Zhang Zhenfeng
2005-11-17
Ad Hall
Ti etchant but not etch SiO2
Ad Hall
2005-11-17
Check out this site.  Transene makes a chemical that will do the trick.

http://www.transene.com/etch_compatibility.html


Ad Hall
StarCryoelectronics
505-424-6454
[email protected]


-----Original Message-----
From: [email protected] [mailto:[email protected]]
On Behalf Of Zhang Zhenfeng
Sent: Wednesday, November 16, 2005 5:08 PM
To: mems-talk
Subject: [mems-talk] Ti etchant but not etch SiO2

Dear All£¬
Do you know which etchant can etch Ti but not SiO2?
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
University Wafer
Mentor Graphics Corporation
Harrick Plasma, Inc.