MEMSnet Home: MEMS-Talk: Al wire-bond
Al wire-bond
2005-11-20
Lung-hao Hu
2005-11-21
Kirt Williams
Thinning Polyimide
2005-11-20
Lung-hao Hu
Al wire-bond
Lung-hao Hu
2005-11-20
Right now I wanna order silicon wafer for wire-bonding.
I wonder that how thick is of Al enough to wire-bond and what the adhesion layer
of Al and its thickness are.

Appreciate it.





Lawrence L.H Hu

Dept.of Mechanical Engineering
Univ.of Colorado Boulder
UCB 427 CO 80309
Email:[email protected]
Tel:303-786-1702(H)
    303-492-0877(Lab)
Fax:303-492-3498
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Mentor Graphics Corporation
University Wafer
Addison Engineering