I wanna use NMP, DMAc, DMSO or DMF to thin polyimide
Is there any one wno can provided me the relationship between the thickness of
thinned polyimide with different ratio of thinner and polyimide, and the spin
speed.

Lawrence L.H Hu

Dept.of Mechanical Engineering
Univ.of Colorado Boulder
UCB 427 CO 80309
Email:[email protected]
Tel:303-786-1702(H)
    303-492-0877(Lab)
Fax:303-492-3498

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
MEMStaff Inc.
Mentor Graphics Corporation
Tanner EDA by Mentor Graphics