A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: peizoelectric materials
peizoelectric materials
2005-11-27
Deepak Kandikuppa
2005-11-29
ckyang
peizoelectric materials
ckyang
2005-11-29
I thought monocrystalline silicon is not a piezoelectic material.
silicon has a symmetrical crystalline structure with covalent bondings. Most
of piezoelec. material lacks a center of symmetry and are with ionic bonds.
(e.g. NaCl)

piezoelectric effect is not equivalent to peizoresistive effect.

hope it helps.

----- Original Message -----
From: "Deepak Kandikuppa" 
To: 
Sent: Monday, November 28, 2005 12:46 AM
Subject: [mems-talk] peizoelectric materials


> hi everyone,
> Can somebody tell me why single crystal silicon is not used as a
> piezoelectric material,but is used as piezoresistive material.
> pls mail me asap..
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
University Wafer
Process Variations in Microsystems Manufacturing
The Branford Group