A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Gold etching
Gold etching
2005-11-30
Sebastien Allard
2005-12-01
Zhang Peng
2005-12-01
Shay Kaplan
2005-12-01
Michael D Martin
2005-12-02
Sebastien Allard
2005-12-02
Bill Moffat
2005-12-02
Sebastien Allard
2005-12-02
David Nemeth
2005-12-05
Manish Hooda
2005-12-02
[email protected]
Gold etching
Bill Moffat
2005-12-02
Why not use lift off.  Dimensional control down to 0.08 microns.


Bill Moffat, CEO
Yield Engineering Systems, Inc.
2185 Oakland Rd., San Jose, CA  95131
(408) 954-8353

-----Original Message-----
From: Sebastien Allard
Sent: Friday, December 02, 2005 4:34 AM
To: General MEMS discussion
Subject: [mems-talk] Gold etching

Hello all,

Unfortunately, TFA gold etch from Transene is in fact a KI+I2 solution.
Just from the safety point of vue, I agree with trying to avoid aqua
regia, but it may be an unfortunate necessary step.

Any thoughts?

Thanks!

Sébastien Allard
LxSix Photonics
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Addison Engineering
MEMS Technology Review
Process Variations in Microsystems Manufacturing