MEMSnet Home: MEMS-Talk: Contact angle of Silicon and SiO2
Contact angle of Silicon and SiO2
2005-12-02
Pradeep Dixit
2005-12-05
Kirt Williams
Argon plasma for gold etching
2005-12-07
Richard Chang
2005-12-08
David Nemeth
Contact angle of Silicon and SiO2
Pradeep Dixit
2005-12-02
Hi all,

Can any one let me know what is the normal contact angle of silicon, thermal
grown SiO2 and LPCVD Si3N4 layer with water ?

After surface treatment like SC1 and RCA cleaning, how much it can
be reduced ?


Many thanks in advance

Pradeep
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
Mentor Graphics Corporation
MEMS Technology Review
The Branford Group