Argon plasma for gold etching
2005-12-07
Richard Chang
2005-12-08
David Nemeth
Argon plasma for gold etching
David Nemeth
2005-12-08
I don't know about your process compatibility, but an iodine based wet etch
(for example Transene TFA, which is KI +I2) is compatible with standard
lithography.  It leaves the exposed gold a little mucked up, which could be
cleaned up with an Argon plasma.

David Nemeth
Senior Engineer
Sophia Wireless, Inc.
14225-C Sullyfield Circle
Chantilly, VA 20151
-----Original Message-----
From: [email protected]
[mailto:[email protected]]On Behalf Of Richard Chang
Sent: Tuesday, December 06, 2005 7:07 PM
To: General MEMS discussion
Subject: [mems-talk] Argon plasma for gold etching


Hi, All,

   I want to use argon plasma to etch away exposed gold.
   My thickness of gold is 1 micron.
   Does anybody have the recipe for the plasma etching, like RF power,
pressure of Argon?
   How long it might take to etch away 1 micron thick gold?
   Thank you.

Best Regards,

Richard


_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk




reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Process Variations in Microsystems Manufacturing
Harrick Plasma, Inc.
MEMS Technology Review