how to seprate electroplated copper from gold seed layer wafer
Pradeep Dixit
2005-12-13
Hi All,

I have electroplated copper (0diameter 100 um) in silicon wafer (300 um) by
'bottom up electroplating'. Bottom wafer has 300 nm thick gold seed layer.
bottom seed layer is bonded with top silicon wafer by photoresist.

Now my problem is - i am not able to seprate these two wafers. Electroplated
copper forms inter-metallalic bond with copper. I tried to seprate these
wafers by putting them in ultrasonic agitator with acetone, but could not
get any success.

Can any one suggest any way/trick to seprate top silcion wafer with bottom
(gold seed layer) wafer ? does gold etchant etch copper also ? If yes, what
is the selectivity ?

Thanks in advance.
Pradeep Dixit
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
MEMS Technology Review
Nano-Master, Inc.
MEMStaff Inc.