roughing of photoresist in RIE
2005-12-13
乔大勇
2005-12-13
Brent Garber
2005-12-13
Nicolas Duarte
2005-12-13
乔大勇
2005-12-13
Nicolas Duarte
roughing of photoresist in RIE
乔大勇
2005-12-13
I am using a RIE etcher to pattern polysilicon with SF6 & O2, and i observed
that
after a long time etching, the color of the photoresist changed and under SEM,
the
smooth surface of photoresist is replaced by a rough surface, would anybody give
an explanation of this phenomenon?


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
University Wafer
Process Variations in Microsystems Manufacturing
The Branford Group