MEMSnet Home: MEMS-Talk: Deep Si etch 8" wafers
Deep Si etch 8" wafers
2005-12-13
Mac McReynolds
2005-12-14
Aditya Bhandare
2005-12-14
Hongtao Wang
Deep Si etch 8" wafers
Mac McReynolds
2005-12-13
Does any one have a source for deep silicon etching on 200mm wafers??  I'm
looking for depths in the range of 100-200µ, large (50µ plus)
features.  Please feel free to contact me directly.

Mac McReynolds
Process Development Manager
Caliper Life Sciences
605 Fairchild Drive
Mountain View, CA 94043-2234
Tel:  650-623-0710
Fax:  650-623-0521
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics
Harrick Plasma, Inc.