Preform thickness in die attach
2005-12-15
Yuan Xie
Photoresist Exposure Dose
2006-01-10
haixinzhu
2006-01-12
Isaac Chan
2006-01-17
Robert Black
Preform thickness in die attach
Yuan Xie
2005-12-15
Hi,

For die attaching (Si substrate to ceramic DIL
package),
what is the suggested thickness for the preform (Au/Si

is used for higher melting point)? Does 0.0021" (2mil)

or 0.001"(1mil) matter? Thanks for any suggestion.

Yuan
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
Process Variations in Microsystems Manufacturing
Nano-Master, Inc.
Addison Engineering