Removing dry resist
2005-12-21
Sven Holmström
2005-12-21
ckyang
2005-12-21
Shile
2005-12-22
Sven Holmström
2005-12-23
Robert Black
2005-12-23
Jesse D Fowler
Removing of Polycarbonate (PC)
2005-12-25
Daniel Park
2005-12-21
Jauniskis, Linas
2005-12-22
Prem Pal
Removing dry resist
Sven Holmström
2005-12-21
Hi

We have a problem regarding the removal of resist.

We have two wafers with memsstructure of aliminum and gold
respectively. We want to release them by etching a sacrificial crome
layer. On top of the crome a protective layer of Shipley's S1813
resist was put to protect the wafers durings transport.

The resist was only softbaked after spinning.

What obviously happened was that the wafers were stored for too long
(around six moths) and now the resist can't be stripped by acetone,
which is what we normally use.

Can anyone here think of any other way to remove the resist? It might
be possible to etch itm but most ethcants etch metals faster than
resists, which would be a big problem.

/Sven Holmström, Koc University, Istanbul
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
The Branford Group
MEMS Technology Review
Tanner EDA by Mentor Graphics