Thin soda lime glass sheet
Carsten Wesselkamp
2005-12-30
The smallest available thickness of soda lime glass (which is produced by
using a special float process) is 0.4 mm. The main reason for this limit is
the manufacturing process (floating), but of course also the small demand
for a lower thickness.

Thinner soda lime glass can be produced by grinding/polishing (e.g. 0.2 mm).
For a quotation please feel free to contact me by e-mail.

Carsten Wesselkamp
Plan Optik AG
Elsoff, Germany
mailto:[email protected]
http://www.planoptik.com




-----Original Message-----
From: [email protected] [mailto:[email protected]]
On Behalf Of Luis Lopes
Sent: Wednesday, December 28, 2005 1:54 PM
To: mems-talk
Subject: [mems-talk] Thin soda lime glass sheet

Hi all,

I’m interest in very thin soda lime glass, 0.2 mm, but the most thin I

can find is 0.5 mm. I don’t know if this is some impossible thickens.
Can any body say something about this?


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Nano-Master, Inc.
Mentor Graphics Corporation
Addison Engineering