Hi all,

I am trying to do electroless copper plating on SU-8 structures. But seems
like there is no reaction occured at all on the su-8 surface. I do see some
copper plated on the backside of my Si substrate, though no copper found on
the front side (the polished side) of the Si substrate.

Does anybody have similar experience? Thanks a lot in advance.

Happy new year!

Chao

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Tanner EDA by Mentor Graphics
Mentor Graphics Corporation
MEMS Technology Review